Problem: Back Ionizer

CauseRemedies
The so-called back ionization is created when
the powder coating is too thick.
Reducing the high-voltage prevents back ionization; this however,
results in a reduction of the powder transfer rate. Back ionization
formation is also dependent on the temperature, and relative
humidity.  With very difficult powders air-conditioning of the
coating area may be necessary. See also “Orange peel”.