Cause | Remedies | |
---|---|---|
Fluidization of the powder has a great influence on the coating quality. | In addition, with difficult powders we recommend to add a vibration of the powder hopper. Retrofitting a pneumatic or electric vibrating table is simple. Remark: GEMA OPTICENTERS ARE NOT PREPARED TO WORK WITH A VIBRATING TABLE. | |
Lumps appear in the fluidized powder, if the powder is stored too long or came into contact with temperatures over 35° C (95° F). | Use new powder and check the storage conditions of the powder. | |
Poor fluidization of the powder can be caused by the fluidizing air being set too low. | Check the fluidizing air setting. |